.Harding
Process
:
Adding 3-5 gram harder to mix silicone emulsion and put in a vacuum glass cover of manual by hand can vacuumized with 3kg Mixxing liquid .Start the machine for 2-4 minutes till the air in the mixing emulsions completely removed.
4.Pouring of Silicone oil & Covering Model
Taking out mixing emulsion and pouring into pad module. Cover a wooden plate on it. There are two kinds of mould, One is Transparence resin mould, The other is PET adsorption mould . Pet adsorption mould is suitable for commonly rubber pads. Transparence resin mould more suitable for making high quality rubber pads.
5. Solidifying silicone Oil
Solidification speed is related with the environment temperature, higher temperature,faster solidificationspeed. Otherwise, in order to expedite solidification speed, please put more hardener into mixing emulsion.
6.Optimizing Hardness
Complete solidification requires 5 hours. Adjust the percentage of silicon oil can adjust the the hardness of rubber pad. Less percentage of silicon oil will produce a harder pad. When you increase the percentage of silicon pad, please add corresponding percentage of hardener. But, too much percentage of silicon oil will affect pad quality negatively. Precision hardness of rubber pad need measure with Shore duromet